BLASTING & PAINTING QUESTION ANSWER Q.1. ) there are 6 types of surface preparation grade in blasting -T/F F Primer is the actual corrosion inhibitor in the paint system T/F T Magnetic temperature gauge used to measure the blasting pressure T/F F blasting pressure should measure without abrasive material in the blasting hose T/F F hypodermic needle gauge used to measure the surface roughness T/F F Hypodermic needle gauge should insert opposite to the air flow T/F hypodermic needle gauge should insert at 31 degree to air flow pipe T/F F smaller the garnet mesh size higher the roughness property T/F F St 3 is a hand tool surface preparation grade by manually T/F F VS % stands for velocity of sound T/F F pigment is related word about garnet type T/F F purpose of intermediate coat to provide natural drainage to the paint system T/F F SA-3 is a 3rd type of surface preparation grade by abrasive material T/F F For black colour paint we use titanium dioxide pigment T/F F There are 5 atmospheric environment condition in the corrosion system T/F F steel is unstable structure in the environment T/F T low durability period require less DFT paint T/F T CM5 atmospheric corrosivity is a urban & industrial environment T/F F blast nozzle control by Deadman's handle T/F painting tip fan width measure at a distance of 10 inch from substrate T/F blasting nozzle NO 5 is require more air pressure than NO 6 T/F F