Introduction To Semiconductor Manufacturing Technology T. S. Chao Dept. of Electrophysics 1/41 1/78 CMOS Process Flow • Overview of Areas in a Wafer Fab – Diffusion (oxidation, deposition and doping) – Photolithography – Etch – Ion Implant – Thin Films – Polish • CMOS Manufacturing Steps • Parametric Testing • 6~8 weeks involve 350-step 2/78 Model of Typical Wafer Flow in a Sub-Micron CMOS IC Fab Wafer Fabrication (front-end) Wafer Start Unpatterned Wafer Completed Wafer Test/Sort Diffusion Thin Films Polish Photo Etch Implant 6 major production areas 3/78 Clean: Types of Contamination and The Problems They Cause • Particles • Metallic Impurities • Organic Contamination • Native Oxides • Electrostatic Discharge • Contamination often leads to a defective chip. Killer defects are those causes of failure where the chip on the wafer fails during electrical test. • It is estimated that 80% of all chip failure are due to killer defects from contamination. 4/78 Wafer Wet-Cleaning Chemicals Contaminant Particles Organics Metallics (not Cu) Name Piranha (SPM) SC-1 (APM) SC-1 (APM) SC-2 (HPM) Piranha (SPM) DHF Chemical Mixture Description (all Cleans are followed by a DI Water Rinse) Sulfuric acid/hydrogen peroxide/DI water H2SO4/H2O2/H2O Ammonium hydroxide/hydrogen peroxide/DI water NH4OH/H2O2/H2O Ammonium hydroxide/hydrogen peroxide/DI water NH4OH/H2O2/H2O Hydrochloric acid/hydrogen peroxide/DI water HCl/H2O2/H2O Sulfuric acid/hydrogen peroxide/DI water H2SO4/H2O2 Hydrofluoric acid/water solution (will not remove copper) Hydrofluoric acid/water solution (will not remove copper) DHF BHF Native Oxides Chemicals Buffered hydrofluoric acid HF/H2O HF/H2O NH4F/HF/H2O 5/78 Typical Wafer Wet-Cleaning Sequence Cleaning Step H2SO4/H2O2 (piranha) UPW rinse (ultrapure water) HF/H2O (dilute HF) UPW rinse NH4OH/H2O2/H2O (SC-1) UPW rinse HF/H2O UPW rinse HCl/H2O2/H2O (SC-2) UPW rinse HF/H2O UPW rinse Drying What it Cleans Organics & metals Rinse Native oxides Rinse Particles Rinse Native oxides Rinse Metals Rinse Native oxides Rinse Dry 6/78 Diffusion: Simplified Schematic of HighTemperature Furnace Temperature controller Thermocouple measurements Gas flow controller Process gas Quartz tube Temperaturesetting voltages Heater 1 Heater 2 Heater 3 Three-zone Heating Elements Pressure controller Exhaust Can do : oxidation, diffusion, deposition, anneals, and alloy 7/78 Dry Oxidation Time (Minutes) Si (solid) + O2 (gas) SiO2 (solid) 10.0 Oxide thickness (mm) (100) Silicon 1.0 0.1 0.01 10 102 103 104 Time (minutes) 8/78 Wet Oxygen Oxidation Gas panel Exhaust Furnace Scrubber Burn box HCl N2 O2 H2 • H2+O2 H2O • Si (solid) + 2H2O SiO2 (solid) + 2H2 • The fast growth rate in wet atmosphere is due to the faster diffusion and higher solubility of water vapor than oxygen in silicon dioxide • Hydrogen molecules produced in the reaction are trapped in oxide, less dense, using heating (annealing) to improve. 9/78 Negative Lithography Ultraviolet light Chrome island on glass mask • Areas exposed to light become crosslinked and resist the developer chemical. Island Exposed area of photoresist Window Photoresist Shadow on photoresist Photoresist Oxide Oxide Silicon substrate Silicon substrate Resulting pattern after the resist is developed. 10/78 Positive Lithography Ultraviolet light Chrome island on glass mask Areas exposed to light are dissolved. Shadow on photoresist Island Window photoresist Photoresist Exposed area of photoresist photoresist Photoresist oxide Oxide oxide Oxide silicon substrate Silicon substrate silicon substrate substrate Silicon Resulting pattern after the resist is developed. 11/78 Eight Steps of Photolithography UV Light HMDS Resist Mask 1) Vapor prime 2) Spin coat 3) Soft bake 4) Alignment and Exposure 5) Post-exposure bake 6) Develop 7) Hard bake 8) Develop inspect 12/78 Photolithography Bay in a Sub-micron Wafer Fab • It is to photograph the image of a circuit pattern onto the photoresist that coats the wafer surface. • Yellow fluorescent does not affect photoresist, but sensitive to UV 13/78 Simplified Schematic of a Photolithography Processing Module Load Station Wafer Cassettes Vapor Prime Resist Coat Develop- Edge-Bead Rinse Removal Transfer Station Wafer Stepper (Alignment/Exposure System) Wafer Transfer System Soft Bake Cool Plate Cool Plate Hard Bake Note: wafers flow from photolithography into only two other areas: etch and ion implant 14/78 Etch: Dissociation • Electron collides with a molecule, it can break the chemical bond and generate free radicals: e + AB A+B+ e • Free radicals have at least one unpaired electron and are chemically very reactive. • Increasing chemical reaction rate • Very important for both etch and CVD. 15/78 Simplified Schematic of Dry Plasma Etcher • The etch process creates a permanent pattern on the wafer in areas not protected by the photoresist pattern • Including: dry etching, wet etching and photoresist stripper • After dry etching: photoresist stripper + wet cleaning Etchant gas entering gas inlet Gas distribution baffle High-frequency energy Anode electrode RF coax cable Photon Electromagnetic field - e Free electron e Glow discharge (plasma) Vacuum gauge Ion sheath - Wafer e Cathode electrode + Chamber wall Positive ion R Radical chemical Vacuum line Flow of byproducts and process gases Exhaust to vacuum pump 16/78 Wet Chemical Isotropic Etch • Etch profile refers to the shape of the sidewall of the etched feature • Isotropic etch profile leads to a undercutting, results in an undesirable loss of the linewidth Isotropic etch - etches in all directions at the same rate Resist Film Substrate 17/78 Anisotropic Etch with Vertical Etch Profile • The rate of etching is on only one direction perpendicular to the wafer surface • There is very little lateral etching activity • This leaves vertical sidewalls, permitting a higher packing density of etched features on the chip • With smaller geometries, the etch profiles have higher aspect ratios • It is difficult to get etchant chemicals in and reaction by-products out of the high-aspect ratio openings Anisotropic etch - etches in only one direction Resist Film Substrate 18/78 Implantation: Common Dopants Used in Semiconductor Manufacturing • Doping is the introduction of a dopant into the crystal structure of a semiconductor material to modify its electronic properties • Dopants are referred to as impurities • Two techniques: thermal diffusion and ion implantation (dominant) Acceptor Dopant Group IIIA (P-Type) Element Atomic Number Semiconductor Group IVA Element Atomic Number Donor Dopant Group VA (N-Type) Element Atomic Number Boron (B) 5 Carbon 6 Nitrogen 7 Aluminum 13 Silicon (Si) 14 Phosphorus (P) 15 Gallium 31 Germanium 32 Arsenic (As) 33 Indium 49 Tin 50 Antimony 51 19/78 General Schematic of an Ion Implanter • • • • Ion source: positive charge Extraction assembly: extract ions Mass Analyzer: form a beam of the desired dopant ions Acceleration column: to attain a high velocity Ion source Plasma Extraction assembly Analyzing magnet Ion beam Acceleration column Process chamber Scanning disk 20/78 Annealing of Silicon Crystal Ion Beam Repaired Si lattice structure and activated dopant-silicon bonds a) Damaged Si lattice during implant b) Si lattice after annealing • Using Furnace or RTA, hot-wall furnace using high temperature causes extensive dopant diffusion and is undesirable • RTA minimizes a phenomenon known as transient enhanced diffusion, to achieve acceptable junction depth control in shallow implants (~150°C/sec) 21/78 Thin Film Metallization Bay 22/78 Simple Parallel Plate DC Diode Sputtering System Cathode (-) Metal target 1) Electric fields create Ar+ ions. + + + + + e- 2) collide with metal target. e- Gas delivery Argon atoms High-energy Ar+ ions e3) Metallic atoms are dislodged from target. Exhaust Plasma Electric field 6) Excess matter is removed from chamber by a vacuum pump. 4) Metal atoms migrate toward substrate. DC diode sputterer 5) Metal deposits on substrate Substrate Anode (+) 23/78 Simplified Schematics of CVD Processing System Gas inlet Capacitivecoupled RF input Process chamber Chemical vapor deposition Wafer Susceptor Exhaust Heat lamps CVD cluster tool 24/78 Schematic of CVD Transport and Reaction 8 Steps 1) Mass transport of reactants CVD Reactor Gas delivery 2) Film precursor reactions 3) Diffusion of gas molecules 4) Adsorption of precursors 7) Desorption of byproducts By-products 5) Precursor diffusion into substrate 8) By-product removal Exhaust 6) Surface reactions Continuous film Substrate 25/78 CVD Reaction • Take place on wafer surface: heterogeneous reaction (surface catalyzed). • Homogeneous reaction: above surface (gas reaction), which is poor adhesion, low-density with high defects • SiH4 SiH2 +H2 ( SiH2 is precursor, it is pyrolysis) • CVD reaction steps are sequential, the slowest step defines the bottleneck 26/78 LPCVD Reaction Chamber for Deposition of Oxides, Nitrides, or Polysilicon Three-zone heating element Pressure gauge Exhaust to vacuum pump Gas inlet Profile thermocouples (internal) Spike thermocouples (external, control) • Limited by surface reaction, flow condition is not important • Films are uniformly deposited on a large number of wafer surface as long as the temperature is tightly controlled • Conformal film coverage on the wafer • Low growth rate than APCVD and need routine maintenance • In-situ clean, using ClF3 or NF3 • 3SiCl2H2 + 4NH3 Si3N4 + 6HCl + 6H2 27/78 Polish Bay in a Sub-micron Wafer Fab • Chemical mechanical planarization (CMP) process is to planarize the top surface of the wafer by lowering the high topography to be level with the lower surface area of the wafer • It combines chemical etching and mechanical abrading to remove layer 28/78 Schematic of Chemical Mechanical Planarization (CMP) Step height: etchback ~ 7000Å vs. CMP ~ 50Å Downforce Wafer carrier Polishing pad Slurry dispenser Wafer Rotating platen • • Polishing slurry CMP achieves wafer planarity by removing high features on the surface more quickly relative to the low feature (high pressure by Preston’s eq.) Both metal and dielectric layers can be removed 29/78 Biasing Circuit for an NMOS Transistor S1 Open gate (no charge) VGG = + 0.7 V Gate Source Drain n+ n+ p-type silicon substrate Lamp (no conduction) VDD = + 3.0 V Figure 3.16 30/78 NMOS Transistor in Conduction Mode S1 VGG = + 0.7 V Positive charge Gate e- ++++++ ++++++ ++++++ Source n+ Drain IDS n+ Holes p-type silicon substrate Lamp e- eVDD = + 3.0 V 31/78 Biasing Circuit for a P-Channel MOSFET S1 Open gate (no charge) VGG = - 0.7 V Gate Source Drain p+ p+ n-type silicon substrate Lamp (no conduction) VDD = -3.0 V 32/78 PMOS Transistor in Conduction Mode S1 Negative charge VGG = - 0.7 V Gate e- ---------------------- Source p+ Drain IDS p+ Electrons n-type silicon substrate Lamp e- eVDD = - 3.0 V 33/78 Schematic of a CMOS Inverter + VDD S G pMOSFET D Input Output D nMOSFET G S - VSS 34/78 Cross-section of CMOS Inverter Interlayer Oxide Metal pMOSFET nMOSFET G +VDD S D D n+ p+ p+ n+ G S n+ -VSS p+ p-well n-type silicon substrate Field oxide 35/78 CMOS Manufacturing Steps 1. Twin-well Implants 14 Passivation layer 2. Shallow Trench Isolation Bonding pad metal ILD-6 3. Gate Structure ILD-5 4. Lightly Doped Drain Implants M-4 13 5. Sidewall Spacer ILD-4 M-3 6. Source/Drain Implants ILD-3 12 7. Contact Formation M-2 11 8. Local Interconnect ILD-2 M-1 9. Interlayer Dielectric to Via-1 Via 10. First Metal Layer 11. Second ILD to Via-2 n+ 12. Second Metal Layer to Via-3 13. Metal-3 to Pad Etch 2 7 ILD-1 9 Poly gate 8 LI metal 10 3 p+ 4 5 LI oxide p+ STI n-well n+ n+ p+ 6 p-well 1 p- Epitaxial layer 14. Parametric Testing p+ Silicon substrate 36/78 n-well Formation • • Epitaxial layer : improved quality and fewer defect In step 2, initial oxide (15 nm) : (1) protects epi layer from contamination, (2) prevents excessive damage to ion/implantation, (3) control the depth of the dopant during implantation • In step 5, anneal: (1) drive-in, (2) repair damage, (3) activation Phosphorus implant Thin Films 2 Polish 3 5 Photoresist 2 1 Diffusion 3 Photo 4 Implant Etch Oxide 4 n-well 5 ~5 um 1 p- Epitaxial layer p+ Silicon substrate (Dia = 200 mm, ~2 mm thick) 37/78 Mask # 1 : N-well formation 38/78 p-well Formation • 2nd mask, this mask is the direct opposite of the n-well implant mask • Boron is 1/3 the mass of P, so 1/3 energy is used. Boron implant Thin Films Polish 1 Photo Etch Oxide Photoresist 1 Diffusion 3 n-well 2 2 Implant p-well 3 p- Epitaxial layer p+ Silicon substrate 39/78 Mask # 2 : P-well formation 40/78 STI Trench Etch STI: shallow trench isolation • • • • Barrier oxide: a new oxide Nitride: (1) protect active region, (2) stop layer during CMP 3rd mask STI etching Selective etching opens isolation regions in the epi layer. +Ions Thin Films 1 2 Diffusion 3 Photo Polish 4 Etch 3 Photoresist 2 1 Nitride 4 Oxide n-well p-well STI trench Implant p- Epitaxial layer p+ Silicon substrate 41/78 Mask # 3: Shallow Trench Isolation formation 42/78 STI Oxide Fill • Liner oxide to improve the interface between the silicon and trench CVD oxide • CVD oxide deposition or spin-on-glass (SOG) Trench fill by chemical vapor deposition Oxide 2 Thin Films 2 Polish Trench CVD oxide Nitride 1 Diffusion Photo Etch 1 n-well p-well Liner oxide Implant p- Epitaxial layer p+ Silicon substrate 43/78 STI Formation 1. Trench oxide polish (CMP): nitride as the CMP stop layer since nitride is harder than oxide 2. Nitride strip: hot phosphoric acid 3. Anti-punch-through and Vth adjustment ion implantation 1 Planarization by chemical-mechanical polishing 1 Thin Films Polish Photo Etch 2 Diffusion STI oxide after polish 2 Nitride strip n-well p-well Liner oxide Implant p- Epitaxial layer p+ Silicon substrate 44/78 Poly Gate Structure Process • • • • Oxide thickness 1.5 ~ 5.0 nm is thermal grown Poly-Si ~ 300 nm is doped and deposited in LPCVD using SiH4 Need Antireflective coating (ARC), very critical The most critical etching step in dry etching 3 Thin Films 1 2 Diffusion 3 Photo Implant Polish 4 Etch Polysilicon deposition 2 1 Photoresist ARC 4 Poly gate etch Gate oxide n-well p-well p- Epitaxial layer p+ Silicon substrate 45/78 Mask # 4 :Poly-Si gate formation 46/78 n- LDD Implant • LDD: lightly doped drain to reduce S/D leakage • Large mass implant (BF2, instead of B, As instead of P) and amorphous surface helps maintain a shallow junction • 5th mask 2 Thin Films Polish Photo Etch 1 Arsenic n- LDD implant Photoresist mask 1 Diffusion n- n-well n- p-well n- 2 Implant p- Epitaxial layer p+ Silicon substrate 47/78 Mask # 5: N- LDD formation 48/78 p- LDD Implant • 6th mask • In modern device, high doped drain is used to reduce series resistance. It called S/D extension BF2 p- LDD implant 2 Thin Films Polish Photo Etch Photoresist Mask Photoresist mask 1 1 1 Diffusion n- p- p- n-well n- n- p-well p- 2 Implant p- Epitaxial layer p+ Silicon substrate 49/78 Mask # 6: P- LDD formation 50/78 Side Wall Spacer Formation • Spacer is used to prevent higher S/D implant from penetrating too close to the channel, cover LDD. • CVD oxide + etch back by anisotropic plasma etching 2 1 Thin Films Polish 1 Spacer etchback by anisotropic plasma etcher +Ions Spacer oxide Side wall spacer 2 Diffusion Photo Implant Etch n- p- p- n-well n- n- p-well p- p- Epitaxial layer p+ Silicon substrate 51/78 n+ Source/Drain Implant • Energy is high than LDD I/I, the junction is deep • 7th mask 2 Thin Films Polish Photo Etch 1 Arsenic n+ S/D implant Photoresist mask 1 Diffusion n+ n-well n+ p-well n+ 2 Implant p- Epitaxial layer p+ Silicon substrate 52/78 Mask # 7: N+ Source/Drain formation 53/78 p+ Source/Drain Implant • 8th mask • Using rapid thermal anneal (RTA) to prevent dopant spreading and to control diffusion of dopant 2 Thin Films Polish Photo Etch Boron p+ S/D implant Photoresist Mask Photoresist mask 1 1 1 Diffusion 3 n+ p+ n-well p+ n+ p-well n+ p+ 2 Implant p- Epitaxial layer p+ Silicon substrate 54/78 Mask # 8 : P+ Source/Drain formation 55/78 Contact Formation • Titanium (Ti) is a good choice for metal contact due to low resistivity and good adhesion • No mask needed, called self-align • Using Ar to sputtering metal • Anneal to form TiSi2, tisilicide • Chemical etching to remove unreact Ti, leaving TiSi2, called selective etching Titanium depostion 1 1 2 3 Thin Films Polish 2 Titanium etch Tisilicide contact formation (anneal) 3 Diffusion Photo Implant Etch n+ p+ n-well p+ n+ p-well n+ p+ p- Epitaxial layer p+ Silicon substrate 56/78 LI Oxide as a Dielectric for Inlaid LI Metal (Damascene) • Damascene: a name doped of year ago from a practice that began thousands ago by artist in Damascus, Syria LI metal LI oxide LI: local interconnection 57/78 LI Oxide Dielectric Formation • Nitride: protect active region • Doped oxide • Oxide polish • 9th mask 2 Doped oxide CVD 3 2 1 Thin Films Polish 1 Nitride CVD 3 Oxide polish 4 LI oxide etch LI oxide 4 Diffusion Photo Implant Etch n-well p-well p- Epitaxial layer p+ Silicon substrate 58/78 Mask # 9: Local Interconnection formation 59/78 LI Metal Formation • Ti/TiN is used: Ti for adhesion and TiN for diffusion barrier • Tungsten (W) is preferred over Aluminum (Al) for LI metal due to its ability to fill holes without leaving voids Diffusion 1 2 3 4 Thin Films Polish Photo Etch Implant Ti/TiN 2 deposition 3 Tungsten deposition 4 LI tungsten polish LI oxide 1 Ti deposition n-well p-well p- Epitaxial layer p+ Silicon substrate 60/78 Via-1 Formation • Interlayer dielectric (ILD): insulator between metal (800nm) • Via: electrical pathway from one metal layer to adjacent metal layer • 10th mask 1 ILD-1 oxide deposition 2 1 Thin Films ILD-1 oxide etch 3 (Via-1 formation) 2 Oxide polish ILD-1 Polish LI oxide 3 Diffusion Photo Implant Etch n-well p-well p- Epitaxial layer p+ Silicon substrate 61/78 Mask # 10: Via-1 formation 62/78 Plug-1 Formation • • • • Ti layer as a glue layer to hold W TiN layer as the diffusion barrier Tungsten (W) as the via CMP W-polish Ti/TiN 2 deposition Diffusion 1 2 3 4 Thin Films Polish Photo Etch Implant 3 Tungsten deposition 1 Ti dep. 4Tungsten polish (Plug-1) ILD-1 LI oxide n-well p-well p- Epitaxial layer p+ Silicon substrate 63/78 SEM Micrographs of Polysilicon, Tungsten LI and Tungsten Plugs Tungsten LI Polysilicon Tungsten plug Mag. 17,000 X Micrograph courtesy of Integrated Circuit Engineering 64/78 Metal-1 Interconnect Formation • Metal stack: Ti/Al (or Cu)/TiN is used • Al(99%) + Cu (1%) is used to improve reliability • 11th mask Ti Deposition 1 TiN 3 deposition 4 Metal-1 etch Al + Cu (1%) 2 deposition 1 2 3 ILD-1 Thin Films Polish LI oxide 4 Diffusion Photo Implant Etch n-well p-well p- Epitaxial layer p+ Silicon substrate 65/78 Common gate for input P+ Source to Vdd N+ Source to ground Common drain or output to next stage Mask # 11: Metal-1 formation 66/78 SEM Micrographs of First Metal Layer over First Set of Tungsten Vias TiN metal cap Metal 1, Al Tungsten plug Mag. 17,000 X Micrograph courtesy of Integrated Circuit Engineering 67/78 Via-2 Formation • • • • Gap fill: fill the gap between metal Oxide deposition Oxide polish 12th mask ILD-2 oxide 2 deposition ILD-2 oxide etch 4 (Via-2 formation) 3 Oxide polish 1 ILD-2 gap fill 1 2 3 Thin Films ILD-1 Polish LI oxide 4 Diffusion Photo Implant Etch n-well p-well p- Epitaxial layer p+ Silicon substrate 68/78 Mask # 12: Via-2 formation 69/78 Plug-2 Formation • Ti/TiN/W • CMP W polish Ti/TiN 2 deposition 1 Ti deposition Diffusion 1 2 3 4 Thin Films Polish Photo Etch Implant Tungsten deposition 3 (Plug-2) Tungsten 4 polish ILD-2 ILD-1 LI oxide n-well p-well p- Epitaxial layer p+ Silicon substrate 70/78 Metal-2 Interconnect Formation • Metal 2: Ti/Al/TiN • ILD-3 gap filling • ILD-3 • ILD-polish • Via-3 etch and via deposition, Ti/TiN/W ILD-3 oxide 3 polish Metal-2 deposition 1 to etch 2 Gap fill 4 Via-3/Plug-3 formation ILD-3 ILD-2 ILD-1 LI oxide n-well p-well p- Epitaxial layer p+ Silicon substrate 71/78 Mask # 13: Metal-2 formation 72/78 Mask # 14: Via-3 formation 73/78 Mask # 15: Metal-3 formation 74/78 CMOS layout (mask 1 to mask 12) 75/78 Full 0.18 mm CMOS Cross Section Passivation layer Bonding pad metal ILD-6 ILD-5 • Passivation layer of nitride is used to protect from moisture, scratched, and contamination • ILD-6 : oxide M-4 ILD-4 M-3 ILD-3 M-2 ILD-2 M-1 Via ILD-1 Poly gate LI oxide LI metal n+ p+ p+ STI n-well n+ n+ p+ p-well p- Epitaxial layer p+ Silicon substrate 76/78 SEM Micrograph of Cross-section of AMD Microprocessor Mag. 18,250 X Micrograph courtesy of Integrated Circuit Engineering 77/78 Wafer Electrical Test using a Micromanipulator Prober (Parametric Testing) • After metal-1 etch, wafer is tested, and after passivation test again • Automatically test on wafer, sort good die (XY position, previous marked with an red ink) • Before package, wafer is backgrind to a thinner thickness for easier slice and heat dissipation Photo courtesy of Advanced Micro Devices 78/78
0
You can add this document to your study collection(s)
Sign in Available only to authorized usersYou can add this document to your saved list
Sign in Available only to authorized users(For complaints, use another form )