Rectification Method of the Minor Cracks in wall plastering
Introduction
There is Minor Crack (Crack width Less than 0.4mm) appear in plaster both vertical and horizontal
Direction even the works were done according to Approved Method of Statement. Therefore it is
proposed to following method to rectify the above work.
Procedure of Rectification of middle Cracks in walls.



Mark the wall crack and Monitor that are further develop.
If not Skim-cote work will continue with applying the 50 mm fiber mesh.
If Crack are Further Develop ,take the Recommendations of a Structural Engineer
Figure 01: Fiber Mesh
Procedure of rectification of crack Located at Beam wall /Colum Wall Joints
This types of Cracks are Mostly Visible at Beam wall Junction. Also some column wall joint this
type of vertical crack are Visible. Therefore following method shall proposed to above issue.




Mark the wall crack and Monitor that are further develop.
If not we are Proposed to Joint sealant (Technical Details of proposed joint Sealant Attach
Herewith)
Surface Preparation and Method of Application Will be done according to manufacture
Specification.
If Crack are Further Develop ,take the Recommendations of a Structural Engineer